1.2085 die steel according to is produced according to the German standard die steel, usually the case pre-hardened (tempered) state delivery, pre-hardened hardness HB280-HB325. scientific moderate adjustment of S content, can improve the steel's easy cutting processing performance, that is, the sulfur system easy cutting die steel.
1, the main chemical composition of the die steel (Wt%)
Element |
C |
Si |
Cr |
Other |
Standard |
0.33 |
0.32 |
16 |
**** |
2, material characteristics: corrosion-resistant, high-alloy, pre-hardened mold steel; can also be used as corrosion-resistant plastic mold; excellent corrosion resistance can reduce mold maintenance workload; can be nitrided, hard chromium plating; Changxiang Special Steel recommends that the steel is not used as a mold insert. 3, process route: EF + LF + VD → hot forging → annealing → milling → pre-hardening → processing mold frame or finishing → real air quenching → surface pressure processing or electroplating or chemical Heat treatment.4、Steel crystallization temperature: 1470℃-1360℃5、Lower than the final forging temperature austenite (A) relative amount.
Temperature |
850℃ |
810℃ |
800℃ |
A phase |
56% |
8% |
0% |
3, heat treatment quenching and hardening temperature: 1000 ℃ -1030 ℃, cooling medium: oil. Vacuum heat treatment can be gas quenching, quenching surface hardness HRC48.
Source:
https://mp.weixin.qq.com/s?__biz=MzA3NjQ1NzEzOQ==&mid=2471411237&idx=1&sn=ac975a347d4e5da6621c631e1ab8cf98&chksm=89daebf9bead62ef22c452baefa8bc7076b86c160d3e39e5597a5a8f9518047ea66b6dec4b56&scene=126&sessionid=1684113010#rd