Long Flow Paths are Necessary to Fill the Large Dies
2022-09-07

Flow Paths for Automotive Tailgate
1.Need for high flow rate when filling the die to prevent premature solidification.
2.Increased casting temperature for correct die filling.
3.Tools for large components must have highly developed thermal control
Source: Kind&Co - //www.kind-co.de/en/
Related News
Principle of mold processing reservation allowance
2023-09-18 9DIN 1.2311 Plastic Mold Steel
2023-09-15 11Selection and Heat Treatment of Die Casting Mold Materials
2023-09-08 15Tooling classification
2023-09-01 24Die steel -1.2738/1.2738HH
2023-08-24 29Mold processing accuracy requirements
2023-08-14 36The main causes of thermal cracks and preventive measures
2023-08-08 39TQ1 Impresses with its Excellent High-Temperature Strength at Higher Working Temperatures
2023-08-03 52Characteristics of die-cast zinc alloy
2023-07-28 56Die Cast Mold
2023-07-25 41Heat treatment - Normalizing
2023-07-12 28Material cracking during heat treatment
2023-06-27 311.4034 tool steel indispensable for saving lives in surgery
2023-06-25 30Kind&Co - Premium steels offer an excellent combination of high toughness and good thermal shock resistance
2023-06-16 40What is high pressure die casting (HPDC)?
2023-06-13 30Classification of forging
2023-05-31 27Undercut molding
2023-05-25 371.2085 Characteristics of die steel
2023-05-15 26Fundamental changes apply for products in future concepts within the automotive die casting
2023-05-12 27What is low pressure die casting (LPDC)?
2023-04-24 38